BC cardboard, there is a single blistering speed over 50, how to do?

Suggest:

One: The overpasses of the flyovers have been piled up. The upper floor has preheated the pits. It should be fine to open the accumulated paper.

Two: To see if there is any problem in the paper in the single-tile machine, and then to increase the tension of the flyover is to increase the suction, try it;

Three: The hot plate temperature is not enough;

Four: Face paper brakes.

V: The gelatinization temperature is too high or the hot plate temperature is too low;

VI: After the production of four layers, the large belt is relatively dry, and the large belt slips and spins, resulting in a mismatch with the roller speed. In other words, the rubber roller turns fast. Solution: 1. Tighten the big belt, 2. Scatter some water on the big belt, 3. Check if the pressure at both ends of the cold section is the same and the light side is easy to appear. 4. If it is not transparent blistering, check the loose side of the preheating cylinder for easy problems.

Information Processing: Carton Street

Baby Care Products

Baby Care Products,Portable Baby Care Organizer,Baby Care Set,Baby Care Activity Set

Dongguan Junkai Packaging Products Co., Ltd , https://www.diystoragecases.com